Popping
Esquema
Jerarquía
procesos que alteran las condiciones > cambios superficiales o estructurales
Descripción
In plaster, the appearance of small, cone-shaped holes up to a quarter inch in diameter; caused by the expansion of lime or foreign material and occurring between three months and up to one year after the plaster has set.
URI original del concepto
Otros términos
- popped [en]